Fse-rubber-and-elastomers-v2.svg (SVG file, nominally 1,220 × 880 pixels, file size: 10 KB)

Summary

Gross heat of combustion of rubbers compared with red oak, from oxygen bomb calorimeter data.

Original illustration for Rubber and elastomers.

  • Alt text: Bar chart: hydrocarbon rubbers about 44 to 46 MJ/kg, tyre 32.6, neoprene 24.3, red oak 20.2 and silicone rubber 15.5 to 16.8 MJ/kg.

Licensing

New drawing by Fire Safety Academy. © Fire Safety Academy.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current08:07, 8 November 2026Thumbnail for version as of 08:07, 8 November 20261,220 × 880 (10 KB)Lisa (talk | contribs)Watermark: Fire Safety Academy logo icon, 70 px, 45 % opacity
07:43, 8 November 2026Thumbnail for version as of 07:43, 8 November 20261,220 × 790 (10 KB)Lisa (talk | contribs)Watermark: Fire Safety Academy logo icon, 70 px, 45 % opacity

The following page uses this file:

Metadata