Contents
Fse-rubber-and-elastomers-v2.svg (SVG file, nominally 1,220 × 880 pixels, file size: 10 KB)
Summary
Gross heat of combustion of rubbers compared with red oak, from oxygen bomb calorimeter data.
Original illustration for Rubber and elastomers.
- Alt text: Bar chart: hydrocarbon rubbers about 44 to 46 MJ/kg, tyre 32.6, neoprene 24.3, red oak 20.2 and silicone rubber 15.5 to 16.8 MJ/kg.
Licensing
New drawing by Fire Safety Academy. © Fire Safety Academy.
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 08:07, 8 November 2026 | 1,220 × 880 (10 KB) | Lisa (talk | contribs) | Watermark: Fire Safety Academy logo icon, 70 px, 45 % opacity | |
| 07:43, 8 November 2026 | 1,220 × 790 (10 KB) | Lisa (talk | contribs) | Watermark: Fire Safety Academy logo icon, 70 px, 45 % opacity |
You cannot overwrite this file.
File usage
The following page uses this file: