Add 4 watermarked NFPA SVG illustrations |
Remove bibliographic source lines from image captions and descriptions |
||
| Line 16: | Line 16: | ||
After the chlorine has gone, the remaining chain carbonises. Between 700 and 750 K (427 to 477 °C) hydrogen is released, and at higher temperatures cross-linking between chains leaves a fully carbonised residue. Oxygen speeds up dehydrochlorination and reduces cross-linking, and above 700 K the char is oxidised and leaves no residue.<ref name="BH-1-126" /> The second stage also produces aromatic hydrocarbons, which form smoke; additives that promote cross-linking reduced smoke formation.<ref name="BH-1-126" /> | After the chlorine has gone, the remaining chain carbonises. Between 700 and 750 K (427 to 477 °C) hydrogen is released, and at higher temperatures cross-linking between chains leaves a fully carbonised residue. Oxygen speeds up dehydrochlorination and reduces cross-linking, and above 700 K the char is oxidised and leaves no residue.<ref name="BH-1-126" /> The second stage also produces aromatic hydrocarbons, which form smoke; additives that promote cross-linking reduced smoke formation.<ref name="BH-1-126" /> | ||
[[File:fse-polyvinyl-chloride-v1.svg|thumb|upright=1.5|alt=Temperature scale with three stages of PVC decomposition: HCl release from about 227 °C, carbonisation from about 427 °C, char oxidation in air above 427 °C.|Decomposition stages of PVC with rising temperature: release of hydrogen chloride by chain stripping, carbonisation of the remaining chain, and oxidation of the char in air | [[File:fse-polyvinyl-chloride-v1.svg|thumb|upright=1.5|alt=Temperature scale with three stages of PVC decomposition: HCl release from about 227 °C, carbonisation from about 427 °C, char oxidation in air above 427 °C.|Decomposition stages of PVC with rising temperature: release of hydrogen chloride by chain stripping, carbonisation of the remaining chain, and oxidation of the char in air.]] | ||
This cross-linking explains why rigid PVC, unlike most thermoplastics, forms a char when it burns.<ref name="MS-2-33" /><ref name="BH-1-123">Beyler and Hirschler (2002), p. 1-123.</ref> CPVC decomposes by the same mechanism but at a much higher temperature. Its residue gives off much less smoke than PVC and is more difficult to burn.<ref name="BH-1-126" /> | This cross-linking explains why rigid PVC, unlike most thermoplastics, forms a char when it burns.<ref name="MS-2-33" /><ref name="BH-1-123">Beyler and Hirschler (2002), p. 1-123.</ref> CPVC decomposes by the same mechanism but at a much higher temperature. Its residue gives off much less smoke than PVC and is more difficult to burn.<ref name="BH-1-126" /> | ||
| Line 32: | Line 32: | ||
The effective heat released depends on combustion conditions. For one set of selected-material values, NUREG/CR-6850 uses a PVC heat of combustion of 16.4 MJ/kg and a combustion efficiency of 0.35, giving an effective value of 5.74 MJ/kg. Its listed heat release rate is 92 kW/m², against 993 kW/m² for polyethylene under the table's assumptions.<ref name="NO-G-24">Nowlen et al. (2005b), p. G-24.</ref> The Australian Fire Safety Verification Method data sheets independently list 5.7 MJ/kg as a bench-scale effective heat of combustion for well-ventilated PVC. These numerically similar values do not establish one value for every PVC formulation or fire.<ref name="ABCB-B2-21">Australian Building Codes Board (2020a), Data Sheet B2, p. 21.</ref> A PVC waiting-room chair with a metal frame reached a peak heat release rate of 270 kW in tests listed in NFPA 921 (2004 edition).<ref name="CU-2-50">NFPA 921 (2004), as cited in Custer (2008), p. 2-50.</ref> | The effective heat released depends on combustion conditions. For one set of selected-material values, NUREG/CR-6850 uses a PVC heat of combustion of 16.4 MJ/kg and a combustion efficiency of 0.35, giving an effective value of 5.74 MJ/kg. Its listed heat release rate is 92 kW/m², against 993 kW/m² for polyethylene under the table's assumptions.<ref name="NO-G-24">Nowlen et al. (2005b), p. G-24.</ref> The Australian Fire Safety Verification Method data sheets independently list 5.7 MJ/kg as a bench-scale effective heat of combustion for well-ventilated PVC. These numerically similar values do not establish one value for every PVC formulation or fire.<ref name="ABCB-B2-21">Australian Building Codes Board (2020a), Data Sheet B2, p. 21.</ref> A PVC waiting-room chair with a metal frame reached a peak heat release rate of 270 kW in tests listed in NFPA 921 (2004 edition).<ref name="CU-2-50">NFPA 921 (2004), as cited in Custer (2008), p. 2-50.</ref> | ||
[[File:fse-polyvinyl-chloride-v3.svg|thumb|upright=1.5|alt=Selected NUREG table values: polyethylene 43.4 MJ/kg, efficiency 0.88, 993 kW/m²; PVC 16.4 MJ/kg, efficiency 0.35, 92 kW/m².|Selected engineering values for polyethylene and PVC under the assumptions of NUREG/CR-6850 Table G-8 | [[File:fse-polyvinyl-chloride-v3.svg|thumb|upright=1.5|alt=Selected NUREG table values: polyethylene 43.4 MJ/kg, efficiency 0.88, 993 kW/m²; PVC 16.4 MJ/kg, efficiency 0.35, 92 kW/m².|Selected engineering values for polyethylene and PVC under the assumptions of NUREG/CR-6850 Table G-8.]] | ||
== Hydrogen chloride and smoke == | == Hydrogen chloride and smoke == | ||
| Line 54: | Line 54: | ||
Additives that bind chlorine change this picture. For compounds of PVC, the plasticiser dioctyl phthalate and calcium carbonate, pyrolysed in nitrogen, the yield fell from 0.221 g/g with 9.0 % calcium carbonate to 0.117 g/g with 28.6 %. For the second compound, with 35.7 % PVC, the maximum yield is 0.357 × 0.583 = 0.208 g/g, so only about 56 % of the chlorine was released as HCl. With potassium carbonate the effect was stronger, and the compound with 32.5 % PVC released only 0.029 g/g, about 15 % of its maximum.<ref name="TE-3-139" /> | Additives that bind chlorine change this picture. For compounds of PVC, the plasticiser dioctyl phthalate and calcium carbonate, pyrolysed in nitrogen, the yield fell from 0.221 g/g with 9.0 % calcium carbonate to 0.117 g/g with 28.6 %. For the second compound, with 35.7 % PVC, the maximum yield is 0.357 × 0.583 = 0.208 g/g, so only about 56 % of the chlorine was released as HCl. With potassium carbonate the effect was stronger, and the compound with 32.5 % PVC released only 0.029 g/g, about 15 % of its maximum.<ref name="TE-3-139" /> | ||
[[File:fse-polyvinyl-chloride-v2.svg|thumb|upright=1.5|alt=Paired bars of maximum and measured HCl yield: pure PVC near 100 %, rigid sheet 94 %, compounds with calcium or potassium carbonate down to 15 %.|Measured hydrogen chloride yields of PVC materials compared with the maximum if all chlorine left as HCl. Fillers that bind chlorine lower the yield | [[File:fse-polyvinyl-chloride-v2.svg|thumb|upright=1.5|alt=Paired bars of maximum and measured HCl yield: pure PVC near 100 %, rigid sheet 94 %, compounds with calcium or potassium carbonate down to 15 %.|Measured hydrogen chloride yields of PVC materials compared with the maximum if all chlorine left as HCl. Fillers that bind chlorine lower the yield.]] | ||
The NFPA handbook explains such results by the formation of solid calcium chloride, which is thermally stable under ordinary fire conditions.<ref name="GB-6-13" /> The equation is therefore an upper bound. Early in decomposition, however, HCl can be released before much carbon has burned, so the yield per unit mass lost can then exceed the stoichiometric value.<ref name="GB-6-13" /> | The NFPA handbook explains such results by the formation of solid calcium chloride, which is thermally stable under ordinary fire conditions.<ref name="GB-6-13" /> The equation is therefore an upper bound. Early in decomposition, however, HCl can be released before much carbon has burned, so the yield per unit mass lost can then exceed the stoichiometric value.<ref name="GB-6-13" /> | ||
HCl is both a potent sensory irritant and a strong pulmonary irritant, and it is the most prominent subject of [[fire toxicity]] studies on halogen acids. Volume fractions as low as 75 to 100 µL/L are extremely irritating to the eyes and upper respiratory tract. ISO 13571 suggests an incapacitating volume fraction of 1,000 µL/L.<ref name="GB-6-16" /> NUREG-1805 adds that concentrations of 1,000 to 2,000 ppm are dangerous even for short exposures.<ref name="IS-B-68">Iqbal and Salley (2004), p. B-68.</ref> | HCl is both a potent sensory irritant and a strong pulmonary irritant, and it is the most prominent subject of [[fire toxicity]] studies on halogen acids. Volume fractions as low as 75 to 100 µL/L are extremely irritating to the eyes and upper respiratory tract. ISO 13571 suggests an incapacitating volume fraction of 1,000 µL/L.<ref name="GB-6-16" /> NUREG-1805 adds that concentrations of 1,000 to 2,000 ppm are dangerous even for short exposures.<ref name="IS-B-68">Iqbal and Salley (2004), p. B-68.</ref> | ||
[[File:fse-polyvinyl-chloride-v4.svg|thumb|upright=1.5|alt=Logarithmic HCl scale showing dated exposure limits, reported human effects, model criteria and separate baboon observations.|Selected historical HCl limits, human effects and animal observations on one concentration scale | [[File:fse-polyvinyl-chloride-v4.svg|thumb|upright=1.5|alt=Logarithmic HCl scale showing dated exposure limits, reported human effects, model criteria and separate baboon observations.|Selected historical HCl limits, human effects and animal observations on one concentration scale.]] | ||
Benedetti and Colonna describe HCl's strong irritation as ordinarily prompting evacuation before toxic effects become dangerous; this presumes that occupants can leave the exposure.<ref name="BC-6-230" /> HCl concentrations can decay on adsorptive surfaces and in water droplets.<ref name="GB-6-13" /> In an unventilated 2.8 m × 2.8 m × 2.4 m room test with burning PVC floor covering, about 50 % of the original chloride ions in the PVC were deposited on the walls.<ref name="TE-3-138" /> | Benedetti and Colonna describe HCl's strong irritation as ordinarily prompting evacuation before toxic effects become dangerous; this presumes that occupants can leave the exposure.<ref name="BC-6-230" /> HCl concentrations can decay on adsorptive surfaces and in water droplets.<ref name="GB-6-13" /> In an unventilated 2.8 m × 2.8 m × 2.4 m room test with burning PVC floor covering, about 50 % of the original chloride ions in the PVC were deposited on the walls.<ref name="TE-3-138" /> | ||
Latest revision as of 08:25, 8 November 2026
Polyvinyl chloride (PVC) is a chlorine-containing thermoplastic polymer with the repeating unit –(CH2–CHCl)–, used both as a rigid, unplasticised material and as a flexible material softened with plasticisers.[1] Together with polyethylene and polypropylene it is one of the most widely used synthetic polymers, and it appears in pipes, siding, flooring, wall coverings, upholstery, roofing and the insulation and jackets of electrical cables.[1][2] Because more than half of its mass is chlorine, PVC behaves differently in fire from most plastics.[3] Rigid PVC burns with difficulty and chars, but plasticisers increase its tendency to burn.[4][5]
When heated, PVC can release much of its chlorine as hydrogen chloride before flaming starts; the temperature and yield depend on its formulation.[2][6] The gas is a strong irritant and is corrosive to metals and electronic equipment, so fires involving PVC can cause damage beyond the flames.[7][8] Some PVC products also have high smoke yields.[9] Fillers and additives change these properties strongly, so the handbook advises testing PVC building products individually.[2]
Composition and grades
The vinyl resins are thermoplastics that exist as a wide variety of polymers and copolymers. Commercial production of the vinyl chloride monomer starts from acetylene or ethylene, and most plants use an oxychlorination process with ethylene. Copolymers of vinyl chloride and vinyl acetate account for a large share of vinyl production.[2] The handbook lists the vinyls among the thermoplastics, the group described in thermoplastics and thermosets.[10] PVC exists in hundreds of individual formulations. It is made as a rigid product for building components and as a flexible, plasticised stock for upholstery and clothing.[2]
Beyler and Hirschler call PVC unique because it is used both rigid (unplasticised) and flexible (plasticised), the flexibility coming from added plasticisers or flexibilisers.[1] Related materials include chlorinated PVC (CPVC), made by further chlorination and with very different physical and fire properties, and polyvinylidene chloride (PVDC).[1] Copolymers with 5 to 20 % vinyl acetate give more flexible stock but keep essentially the properties of PVC.[2] Typical applications of flexible and rigid vinyls include car seat covers, floor mats, shower curtains, window shades, wrappings, bottles, adhesives, flooring, siding, piping, wiring and swimming pools.[2]
The two grades differ markedly in their properties. For rigid PVC the handbook lists a glass transition temperature of 81 °C, a softening temperature of 90 °C and a melting range of 210 to 230 °C. For a flexible grade the values are −25 °C, 75 to 115 °C and 150 to 185 °C.[11] An SFPE table gives 5 to 15 % crystallinity and a glass transition of 80 to 85 °C, but prints "75–105 (212)" in its crystalline melting column for PVC. That entry is ambiguous and conflicts with the rigid-PVC range in the NFPA table.[12]
In processing, flexible PVC for packaging is compounded in high-intensity mixers, where frictional heat lets the resin absorb plasticisers and stabilisers at 88 to 116 °C (190 to 240 °F).[13] Foamed PVC for clothing and upholstery, called "expanded vinyl", is usually blown with azodicarbonamide, which releases nitrogen above 149 °C (300 °F).[14] These processing temperatures are distinct from the ignition values discussed below.
Thermal decomposition
The decomposition of PVC is dominated by chain stripping, in which the chlorine atoms attached to the polymer chain are removed as hydrogen chloride (HCl). In simple terms, each –CH2–CHCl– unit gives up one molecule of HCl and leaves a double bond in the chain.[15] According to Beyler and Hirschler, HCl is evolved nearly quantitatively between 500 and 550 K (227 to 277 °C). The temperature at which measurable release starts depends heavily on the stabiliser package: commercial PVC compounds released no HCl below about 520 K (247 °C) and showed a dehydrochlorination stage from 600 K (327 °C).[16] Common stabilisers are soaps of zinc, cadmium, lead, calcium and barium, and organotin compounds.[16]
After the chlorine has gone, the remaining chain carbonises. Between 700 and 750 K (427 to 477 °C) hydrogen is released, and at higher temperatures cross-linking between chains leaves a fully carbonised residue. Oxygen speeds up dehydrochlorination and reduces cross-linking, and above 700 K the char is oxidised and leaves no residue.[16] The second stage also produces aromatic hydrocarbons, which form smoke; additives that promote cross-linking reduced smoke formation.[16]
This cross-linking explains why rigid PVC, unlike most thermoplastics, forms a char when it burns.[5][17] CPVC decomposes by the same mechanism but at a much higher temperature. Its residue gives off much less smoke than PVC and is more difficult to burn.[16]
The sources differ on when HCl release begins. The NFPA handbook states that HCl is readily evolved at about 225 to 275 °C (437 to 527 °F).[6] Tewarson, in the SFPE Handbook, reports that release can start at temperatures as low as about 100 °C, with HCl the main effluent up to about 200 to 220 °C. The release of HCl leaves double bonds in the polymer and is followed by carbon monoxide and aromatic and unsaturated hydrocarbons such as benzene and toluene.[18]
Ignition and burning behaviour
Polymers that contain halogen atoms, such as PVC, burn with difficulty, but adding plasticisers increases their tendency to burn.[4] The fire properties of plasticised PVC are therefore determined to a large extent by the plasticiser.[2] Unplasticised PVC softens as it burns and produces white smoke and acrid, possibly corrosive fumes.[2]
ASTM D2863 measures the minimum oxygen concentration needed to support candle-like combustion of a plastic, the oxygen index.[19] For PVC the handbook lists oxygen index values of 37.1 to 49, and for CPVC 45 to 60.[20] Air contains only about one-fifth oxygen, so PVC needs an atmosphere considerably richer in oxygen than air to keep burning in that test.[21] PVC is thus an unusual case among plastics in fire.
The ignition data vary with source and test. Table 6.17.7 of the NFPA handbook gives PVC a density of 1,305 kg/m³ and a minimum radiant flux for ignition of 21 kW/m². It lists an ignition temperature of 780 K (507 °C) and an effective heat of gasification of 1.7 to 2.5 MJ/kg.[9] Much lower ignition temperatures are used in engineering calculations: 218 °C for PVC cables in NUREG/CR-6850 and 220 °C for a PVC laminate in a handbook example.[22][23] In that example, a 1 mm thick laminate with a density of 1,450 kg/m³ and a heat capacity of 0.84 kJ/(kg·°C) is exposed to 50 kW/m². Treating the thin sheet as uniformly heated and assuming all incident flux is absorbed with no losses gives an estimated ignition time of about 5 s.[23]
The heat released by PVC is low for a plastic. The handbook gives a net heat of combustion of 16.89 MJ/kg for rigid PVC and 24.70 MJ/kg for a flexible grade, about 1.5 times as much.[11] The International Fire Engineering Guidelines give 17 MJ/kg, and Introduction to Fire Safety Engineering gives 18 MJ/kg for PVC roofing.[24][25]
The effective heat released depends on combustion conditions. For one set of selected-material values, NUREG/CR-6850 uses a PVC heat of combustion of 16.4 MJ/kg and a combustion efficiency of 0.35, giving an effective value of 5.74 MJ/kg. Its listed heat release rate is 92 kW/m², against 993 kW/m² for polyethylene under the table's assumptions.[26] The Australian Fire Safety Verification Method data sheets independently list 5.7 MJ/kg as a bench-scale effective heat of combustion for well-ventilated PVC. These numerically similar values do not establish one value for every PVC formulation or fire.[27] A PVC waiting-room chair with a metal frame reached a peak heat release rate of 270 kW in tests listed in NFPA 921 (2004 edition).[28]
Hydrogen chloride and smoke
Polymers that contain halogens form halogen acids during pyrolysis. These acids are not oxidised further, so they can be produced even without flaming. Conversion of available chlorine into HCl can approach completion, but fillers that bind chlorine lower the yield.[6] Much of the chlorine in PVC can be released as hydrogen chloride.[2] The largest possible yield can therefore be estimated from the chlorine content of the material. If all chlorine leaves as HCl, the yield per unit mass of material follows from the mass fraction of chlorine and the ratio of the molar masses of HCl and chlorine:
| Symbol | Description | Unit |
|---|---|---|
| Maximum (stoichiometric) yield of hydrogen chloride | g/g | |
| Mass fraction of chlorine in the material | – | |
| Molar mass of hydrogen chloride, 36.46 | g/mol | |
| Molar mass of chlorine, 35.45 | g/mol |
For pure PVC, the repeating unit C2H3Cl has a molar mass of 62.50 g/mol, calculated from the atomic weights of carbon (12.01), hydrogen (1.01) and chlorine (35.45).[3][11] Its chlorine fraction is 35.45/62.50 = 0.567, and the maximum HCl yield is 36.46/62.50 = 0.583 g/g. Tewarson's compilation shows measured HCl yields of 0.500 to 0.584 g/g for PVC homopolymers, so nearly all the chlorine was released as HCl. A rigid PVC sheet with 49.3 % chlorine has a maximum yield of 0.493 × 36.46/35.45 = 0.507 g/g and gave 0.479 g/g in air, about 94 % of the maximum.[29]
Additives that bind chlorine change this picture. For compounds of PVC, the plasticiser dioctyl phthalate and calcium carbonate, pyrolysed in nitrogen, the yield fell from 0.221 g/g with 9.0 % calcium carbonate to 0.117 g/g with 28.6 %. For the second compound, with 35.7 % PVC, the maximum yield is 0.357 × 0.583 = 0.208 g/g, so only about 56 % of the chlorine was released as HCl. With potassium carbonate the effect was stronger, and the compound with 32.5 % PVC released only 0.029 g/g, about 15 % of its maximum.[29]
The NFPA handbook explains such results by the formation of solid calcium chloride, which is thermally stable under ordinary fire conditions.[6] The equation is therefore an upper bound. Early in decomposition, however, HCl can be released before much carbon has burned, so the yield per unit mass lost can then exceed the stoichiometric value.[6]
HCl is both a potent sensory irritant and a strong pulmonary irritant, and it is the most prominent subject of fire toxicity studies on halogen acids. Volume fractions as low as 75 to 100 µL/L are extremely irritating to the eyes and upper respiratory tract. ISO 13571 suggests an incapacitating volume fraction of 1,000 µL/L.[7] NUREG-1805 adds that concentrations of 1,000 to 2,000 ppm are dangerous even for short exposures.[30]
Benedetti and Colonna describe HCl's strong irritation as ordinarily prompting evacuation before toxic effects become dangerous; this presumes that occupants can leave the exposure.[8] HCl concentrations can decay on adsorptive surfaces and in water droplets.[6] In an unventilated 2.8 m × 2.8 m × 2.4 m room test with burning PVC floor covering, about 50 % of the original chloride ions in the PVC were deposited on the walls.[18]
PVC can have a high smoke potential. The handbook lists a specific extinction area of 1,100 to 1,400 m²/kg and a soot yield of 0.23 kg/kg.[9] The Australian data sheets give 0.172 kg/kg for well-ventilated bench-scale tests, and Introduction to Fire Safety Engineering gives 0.14 kg/kg.[27][31] These values come from different sources and test contexts; the sources do not isolate the cause of their spread.
Corrosion and non-thermal damage
Severe corrosion damage to sensitive electronic equipment and to metal surfaces can occur after fires involving PVC.[32] HCl and the other acid gases in smoke are especially harmful to electronics. Unless the equipment is close to the fire, however, HCl deposits on walls and lowers the concentration to which the equipment is exposed. The CFAST model in the HAZARD I package contains a routine for this decay.[33] The 2008 handbook describes prompt ventilation, rinsing or dilute-ammonia treatment followed by rinsing as possible post-fire cleaning measures for exposed equipment.[8]
Deposition depends on the surface. Tewarson reports that HCl deposition on wet filter paper was almost four times that on dry paper.[18] The same chemistry offers an early warning. The release of HCl from PVC wire insulation is a fuel-specific fire signature that may be particularly valuable for fire detection in telecommunications facilities, although of little use in general applications.[34] Fuels that contain chlorine also produce chlorine gas as well as HCl.[35]
Electrical cables
PVC is a common material for cable insulation and jackets, so its behaviour matters when it is involved in a cable fire. In US nuclear power plants, cables that have not passed the IEEE 383 flammability test usually have polyethylene and PVC insulation.[36] These are the two predominant thermoplastic cable materials.[37] For screening in US nuclear power plant fire risk analysis, NUREG/CR-6850 assumes that thermoplastic cables are damaged or ignited at 205 °C (400 °F) or at a radiant heat flux of 6 kW/m². For thermoset cables the criteria are 330 °C and 11 kW/m².[38]
Bench-scale data show the same difference. NUREG-1805 lists critical heat fluxes of 13 to 25 kW/m² and thermal response parameters of 156 to 341 kW·s1/2/m² for PVC/PVC power cables.[39] In an example from the SFPE Handbook, a polyethylene/PVC cable had a fire propagation index of 29, indicating accelerating fire propagation, against 4 for a cross-linked polyolefin cable.[40] In an illustrative NUREG/CR-6850 tray calculation that assumes a 2 mm heating distance and 70 kW/m² incident flux, the recommended spread rates are 0.9 mm/s for PVC cable and 0.3 mm/s for cross-linked polyethylene cable.[41] Measured HCl yields of PVC cable jackets range from 0.277 to 0.408 g/g.[29]
Some very severe fires in electric generating plants involved PVC-jacketed cable. One was the 1975 fire in the cable spreading room of the Browns Ferry nuclear power plant, where a candle flame ignited a polyurethane penetration seal and the fire spread to the grouped cables. It caused $302.93 million in property damage, in 2007 US dollars, and an outage of 1.5 years.[42]
Classification and use in building services
In the United States, NFPA standards as described by Golinveaux (2008) classify plastics for sprinkler protection of storage. Highly plasticised PVC, such as coated fabric or unsupported film, is a Group A plastic, the most hazardous group. Rigid or lightly plasticised PVC, such as pipe and pipe fittings, belongs to Group C, which behaves like a Class III commodity.[43] Ouellette likewise notes that unplasticised PVC can be protected like an ordinary Class III commodity, whereas plasticised PVC is among the thermoplastics that present a fire hazard in storage.[44]
CPVC has been used for sprinkler piping. In the United States it was introduced in 1986 and listed for systems complying with NFPA 13D and for NFPA 13 systems in light-hazard occupancies. As described in the 2008 handbook, the pipe must meet ASTM F442 and be specifically listed. It is limited to NFPA 13D, 13R and light-hazard NFPA 13 systems and to wet systems, with limits for dry-pipe and preaction systems. It must be installed behind a thermal barrier, unless it is used with listed residential sprinklers or with quick-response sprinklers within 203 mm (8 in.) of the ceiling.[45]
In upholstery, PVC-coated fabrics made up 5 % of furniture cover fabrics in a 1997 US survey.[46] PVC is listed with wool as a cover fabric of high resistance to cigarette ignition.[47] The good ignition resistance of PVC does not remove its other hazards. Its smoke, its HCl and the corrosion that follows mean that the assessment of a PVC product has to consider more than whether it ignites.[2][32]
See also
Notes
- ↑ 1.0 1.1 1.2 1.3 Beyler and Hirschler (2002), p. 1-112.
- ↑ 2.00 2.01 2.02 2.03 2.04 2.05 2.06 2.07 2.08 2.09 2.10 Benedetti and Colonna (2008), p. 6-222.
- ↑ 3.0 3.1 Drysdale (2008), pp. 2-14–2-15.
- ↑ 4.0 4.1 Gann and Bryner (2008), p. 6-12.
- ↑ 5.0 5.1 Madrzykowski and Stroup (2008), p. 2-33.
- ↑ 6.0 6.1 6.2 6.3 6.4 6.5 Gann and Bryner (2008), p. 6-13.
- ↑ 7.0 7.1 Gann and Bryner (2008), p. 6-16.
- ↑ 8.0 8.1 8.2 Benedetti and Colonna (2008), p. 6-230.
- ↑ 9.0 9.1 9.2 Babrauskas (2008a), p. 6-283.
- ↑ Benedetti and Colonna (2008), p. 6-210.
- ↑ 11.0 11.1 11.2 Babrauskas (2008a), p. 6-279.
- ↑ Beyler and Hirschler (2002), p. 1-113.
- ↑ Ouellette (2008), p. 9-58.
- ↑ Ouellette (2008), p. 9-62.
- ↑ Beyler and Hirschler (2002), p. 1-118.
- ↑ 16.0 16.1 16.2 16.3 16.4 Beyler and Hirschler (2002), p. 1-126.
- ↑ Beyler and Hirschler (2002), p. 1-123.
- ↑ 18.0 18.1 18.2 Tewarson (2002), p. 3-138.
- ↑ Hirschler (2008a), p. 6-58.
- ↑ Babrauskas (2008a), p. 6-282.
- ↑ Drysdale (2008), p. 2-17.
- ↑ Nowlen et al. (2005b), p. R-6.
- ↑ 23.0 23.1 Budnick et al. (2008), p. 3-159.
- ↑ National Research Council of Canada et al. (2005), p. 3.3-6.
- ↑ Van Rossum (2027), §4.4.
- ↑ Nowlen et al. (2005b), p. G-24.
- ↑ 27.0 27.1 Australian Building Codes Board (2020a), Data Sheet B2, p. 21.
- ↑ NFPA 921 (2004), as cited in Custer (2008), p. 2-50.
- ↑ 29.0 29.1 29.2 Tewarson (2002), p. 3-139.
- ↑ Iqbal and Salley (2004), p. B-68.
- ↑ Karlsson and Quintiere (2000) and Tewarson (1988), as cited in Van Rossum (2027), §6.2.
- ↑ 32.0 32.1 Benedetti and Colonna (2008), p. 6-225.
- ↑ Hurley and Bukowski (2008), p. 3-133.
- ↑ Custer and Milke (2008), p. 2-76.
- ↑ Custer and Milke (2008), p. 2-77.
- ↑ Nowlen et al. (2005b), p. R-1.
- ↑ Nowlen et al. (2005b), p. H-8.
- ↑ Nowlen et al. (2005b), p. H-1.
- ↑ Iqbal and Salley (2004), p. 6-6.
- ↑ Tewarson (2002), p. 3-93.
- ↑ Nowlen et al. (2005b), p. R-7.
- ↑ Sheridan (2008), p. 9-187.
- ↑ Golinveaux (2008), pp. 16-73–16-74.
- ↑ Ouellette (2008), p. 9-63.
- ↑ Huggins (2008), pp. 16-42–16-43.
- ↑ Babrauskas (2008b), p. 6-110.
- ↑ Babrauskas (2008b), p. 6-125.
References
- Australian Building Codes Board. (2020a). Data sheets: Fire Safety Verification Method (Handbook annex, Print version 1.1).
- Babrauskas, V. (2008a). Tables and charts. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 6-269–6-294). National Fire Protection Association.
- Babrauskas, V. (2008b). Upholstered furniture and mattresses. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 6-103–6-128). National Fire Protection Association.
- Benedetti, R. P., & Colonna, G. R. (2008). Polymeric materials. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 6-209–6-231). National Fire Protection Association.
- Beyler, C. L., & Hirschler, M. M. (2002). Thermal decomposition of polymers. In P. J. DiNenno, D. Drysdale, C. L. Beyler, W. D. Walton, R. L. P. Custer, J. R. Hall Jr., & J. M. Watts Jr. (Eds.), SFPE handbook of fire protection engineering (3rd ed., pp. 1-110–1-131). National Fire Protection Association; Society of Fire Protection Engineers.
- Budnick, E. K., Hunt, S. P., & Wright, M. T. (2008). Closed form enclosure fire calculations. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 3-145–3-166). National Fire Protection Association.
- Custer, R. L. P. (2008). Dynamics of compartment fire growth. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 2-49–2-58). National Fire Protection Association.
- Custer, R. L. P., & Milke, J. A. (2008). Fundamentals of fire detection. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 2-75–2-78). National Fire Protection Association.
- Drysdale, D. (2008). Physics and chemistry of fire. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 2-3–2-20). National Fire Protection Association.
- Gann, R. G., & Bryner, N. P. (2008). Combustion products and their effects on life safety. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 6-11–6-34). National Fire Protection Association.
- Golinveaux, J. E. (2008). Sprinkler systems for storage facilities. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 16-71–16-89). National Fire Protection Association.
- Hirschler, M. M. (2008a). Concepts and protocols of fire testing. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 6-35–6-60). National Fire Protection Association.
- Huggins, R. (2008). Automatic sprinkler systems. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 16-29–16-53). National Fire Protection Association.
- Hurley, M. J., & Bukowski, R. W. (2008). Fire hazard analysis techniques. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 3-121–3-134). National Fire Protection Association.
- Iqbal, N., & Salley, M. H. (2004). Fire Dynamics Tools (FDTs): Quantitative fire hazard analysis methods for the U.S. Nuclear Regulatory Commission Fire Protection Inspection Program (NUREG-1805). U.S. Nuclear Regulatory Commission, Office of Nuclear Reactor Regulation.
- Madrzykowski, D., & Stroup, D. W. (2008). Flammability hazard of materials. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 2-31–2-48). National Fire Protection Association.
- National Research Council of Canada, International Code Council, Department of Building and Housing, & Australian Building Codes Board. (2005). International fire engineering guidelines (2005 ed.). Australian Building Codes Board.
- Nowlen, S. P., Najafi, B., Wyant, F. J., Forester, J., Kazarians, M., Kolaczkowski, A., Joglar, F., Funk, D., Hannaman, G., & Anoba, R. (2005b). EPRI/NRC-RES fire PRA methodology for nuclear power facilities: Vol. 2. Detailed methodology (NUREG/CR-6850; EPRI 1011989). Electric Power Research Institute; U.S. Nuclear Regulatory Commission, Office of Nuclear Regulatory Research.
- Ouellette, G. (2008). Plastics industry and related process hazards. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 9-53–9-65). National Fire Protection Association.
- Sheridan, D. J. (2008). Electric generating plants. In A. E. Cote, C. C. Grant, J. R. Hall Jr., & R. E. Solomon (Eds.), Fire protection handbook (20th ed., pp. 9-179–9-189). National Fire Protection Association.
- Tewarson, A. (2002). Generation of heat and chemical compounds in fires. In P. J. DiNenno, D. Drysdale, C. L. Beyler, W. D. Walton, R. L. P. Custer, J. R. Hall Jr., & J. M. Watts Jr. (Eds.), SFPE handbook of fire protection engineering (3rd ed., pp. 3-82–3-161). National Fire Protection Association; Society of Fire Protection Engineers.
- Van Rossum, E. (2027). Introduction to Fire Safety Engineering. Fire Safety Academy.