Time to electrical failure of cables exposed to hot gas, as tabulated for US nuclear plant screening. Thermoplastic cables fail at lower temperatures and sooner. Based on Iqbal and Salley (2004), pp. A-16, A-18.
Time to electrical failure of cables exposed to hot gas, as tabulated for US nuclear plant screening. Thermoplastic cables fail at lower temperatures and sooner.


Original illustration for [[Cable fire]].
Original illustration for [[Cable fire]].

Latest revision as of 08:43, 13 November 2026

Summary

Time to electrical failure of cables exposed to hot gas, as tabulated for US nuclear plant screening. Thermoplastic cables fail at lower temperatures and sooner.

Original illustration for Cable fire.

  • Alt text: Line chart of time to cable failure against exposure temperature, thermoplastic from 30 minutes at 205 °C and thermoset from 28 minutes at 330 °C

Licensing

New drawing by Fire Safety Academy. © Fire Safety Academy.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current13:13, 12 November 2026Thumbnail for version as of 13:13, 12 November 2026864 × 860 (10 KB)Peter (talk | contribs)Watermark: Fire Safety Academy logo icon, 70 px, 45 % opacity

The following page uses this file:

Metadata